AVERTISSEMENT : Le chatbot Graph n'est pas programmé pour fournir des réponses explicites ou catégoriques à vos questions. Il transforme plutôt vos questions en demandes API qui sont distribuées aux différents services informatiques officiellement administrés par l'EPFL. Son but est uniquement de collecter et de recommander des références pertinentes à des contenus que vous pouvez explorer pour vous aider à répondre à vos questions.
Two-step spatially delineated growth of copper lines from a solid copper formate layer on a surface is demonstrated. In the first step, a localized platinum film, less than 10 .ANG. high, is deposited. Subsequently the whole surface is covered by a few mic ...
The aim of this research project is to study the deposition of thermal atoms and small ionised clusters on well defined surfaces. For this, an installation has been developed at the Institut de Physique Expérimentale to produce mass selected ionic metal cl ...
Thin, hydrogenated silicon and carbon containing films have been deposited by the siliconization procedure on targets made from some metal alloys, pure metals, graphite and Si single crystal. The deposits were investigated by electron microprobe and surfac ...
The rate of photolytic laser chem. vapor deposition (LCVD) of Pt from its bishexafluoroacetylacetonate precursor is measured as a function of the light intensity, the wavelength, the precursor pressure, and the laser beam diam. at the surface. The waveleng ...
The evolution of the argon metastable states density has been studied by absorption spectroscopy in power-modulated plasmas of argon and a mixture of 4% silane in argon. A small concentration of silane suppresses the argon metastable states density by mole ...
Hydrogenated amorphous silicon has been prepared at a plasma excitation frequency in the very-high-frequency band at 70 MHz with the glow discharge technique at substrate temperatures between 280 and 50-degrees-C. The structural properties have been studie ...
The microstructure and chemical composition of sputtered thin films are strongly correlated with the deposition conditions. In the present work, we report the investigation of the film composition by electron probe microanalysis and photoemission experimen ...
a-Si:H films were prepared using pure silane in the temperature range from 200 degrees C up to 400 degrees C by the very high frequency glow discharge (VHF-GD) technique. During deposition a He/Ne laser beam directed across the discharge monitored powder f ...
Particulate contamination produced during plasma-assisted deposition of amorphous silicon devices can be responsible for reduced quality and yield. The threshold for powder formation imposes an upper limit on the radio frequency (rf) power and hence the de ...