Intrinsic stress measurements were carried out on hydrogenated amorphous silicon (a-Si:H) films deposited with different excitation frequencies (13.56-70 MHz), by plasma-enhanced chemical vapor deposition. It was observed that films deposited at 70 MHz hav ...
1992