DISCLAIMER: The Graph Chatbot is not programmed to provide explicit or categorical answers to your questions. Rather, it transforms your questions into API requests that are distributed across the various IT services officially administered by EPFL. Its purpose is solely to collect and recommend relevant references to content that you can explore to help you answer your questions.
A set of constitutive equations describing the plasticity of semiconductors is compared with the results of mechanical tests. Constant strain-rate compression tests are interrupted before the peak of the initial multiplication yield point, i.e. at the mome ...
The development of a conceptual framework to test different viscoelastic constitutive laws is presented. This framework has the advantage of satisfying a priori the thermodynamic restrictions and is valid for large deformations. In addition, the different ...
A new criterion for the appearance of hot tears in metallic alloys is proposed. Based upon a mass balance performed over the liquid and solid phases, it accounts for the tensile deformation of the solid skeleton perpendicular to the growing dendrites and f ...
Hot tear is one of the most serious defect which a casting can suffer. It represents a major limitation to the production of foundry cast parts and to the productivity of continuous casting processes such as the direct chiil casting of aluminium alloys. As ...
An assessment of the true stress-true strain relationship has been done by means of tensile and small ball punch tests on austenitic and tempered martensitic steel at room temperature. A finite element model was developed and validated to calculate the for ...
Modeling of the constitutive behavior was undertaken for Fe- Cr-C tempered martensitic alloys. Tensile tests were carried out at room temperature and constant nominal strain rate. In order to obtain a fully martensitic structure with different prior austen ...