Hot tearing in polycrystalline Ni-based IN738LC superalloy: Influence of Zr content
Related publications (35)
Graph Chatbot
Chat with Graph Search
Ask any question about EPFL courses, lectures, exercises, research, news, etc. or try the example questions below.
DISCLAIMER: The Graph Chatbot is not programmed to provide explicit or categorical answers to your questions. Rather, it transforms your questions into API requests that are distributed across the various IT services officially administered by EPFL. Its purpose is solely to collect and recommend relevant references to content that you can explore to help you answer your questions.
Mo-Ti alloys form solid solutions over a wide range of compositions, with lattice misfit parameters increasing significantly with titanium content. This indicates a strong increase in the critical stress for edge dislocation motion. Here, we probe the tran ...
We study the creep behavior of Cu64Zr36 glass-crystal nanocomposites under elastostatic loading conditions in molecular dynamics simulations. By manipulating the glass-crystal interfaces of a precipitation-annealed glass containing Laves-type crystallites, ...
The mechanical response of modern alloys results from a complex interplay between existing microstructure and its evolution with time under stress. To unravel these processes, in situ approaches intrinsically have a critical advantage to explore the basic ...
Laser powder bed fusion (LPBF) was used to consolidate powders of a Ni-Cr-Fe-Mo alloy (Hastelloy X) blended with 1 wt% Y2O3 nanometric powders. The nearly-dense, crack-free specimens, with and without oxide dispersion strengthening (ODS), exhibit high-aspe ...
During solidification of metallic alloys, coalescence leads to the formation of solid bridges between grains or grain clusters when both solid and liquid phases are percolated. As such, it represents a key transition with respect to the mechanical behavior ...
Additive manufacturing offers the opportunity to produce complex geometries from novel alloys with improved properties. Adapting conventional alloys to the process-specific properties can facilitate rapid implementation of these materials in industrial pra ...
The formation and growth of cracks by irradiation assisted stress corrosion cracking (IASCC) in light water reactor internals is a critical issue for a safe long-term operation of nuclear power plants. The IASCC susceptibility at relatively low dose is dom ...
The detrimental effects of the H on the mechanical properties of the metals are known for more than a century. One of the most important degradation mechanisms is H embrittlement (HE). In this thesis, we examined a few famous proposed mechanisms in the fie ...
Oxide Dispersed Strengthened (ODS) ferritic stainless steels present well-known fine grains microstructures where dislocation movement is hindered by a dense precipitation of nano-oxides particles. Previous research, on the thermomechanical behavior at hig ...
Oxide dispersion strengthened (ODS) steels are very promising materials for nuclear applications. In thispaper, the hot working behavior of ODS ferritic steels, consolidated by hot extrusion, is studied through torsion tests. Three ODS steels are produced ...