Mechanical behavior of aluminum-silicon nanocomposites: A molecular dynamics study
Graph Chatbot
Chat with Graph Search
Ask any question about EPFL courses, lectures, exercises, research, news, etc. or try the example questions below.
DISCLAIMER: The Graph Chatbot is not programmed to provide explicit or categorical answers to your questions. Rather, it transforms your questions into API requests that are distributed across the various IT services officially administered by EPFL. Its purpose is solely to collect and recommend relevant references to content that you can explore to help you answer your questions.
The three-point bending test by Kolsky-bar apparatus is a convenient technique to test the dynamic fracture properties of materials. This paper presents detailed three-dimensional finite element simulations of a silicon particle reinforced aluminum (SiCp/A ...
Molecular simulations using the quasicontinuum method are performed to understand the mechanical response at the nanoscale of grain boundaries (GBs) under simple shear. The energetics and mechanical strength of 18 Sigma (I 10) symmetric tilt GBs and two Si ...
Al-Cu matrix composites with a high volume fraction of alumina particles (41-62%) prepared by gas-pressure infiltration are characterized in tension and chevron-notch fracture testing before and after heat-treatment. Their mechanical behaviour is shown to ...
At early age, ultra high performance fibre reinforced concretes (UHPFRC)undergo significant volumes changes (thermal deformation and autogenous shrinkage)related to their composition. These deformations can be restrained by different elements respective to ...
In this paper, we use the established cohesive element method to investigate the probabilistic failure of a model ceramic system under dynamic tensile loading. Monte-Carlo simulations are performed to calculate the fracture strength of a monolithic silicon ...
A process of self-assembly induced by electro-chemical etching was used to produce nano and micrometer scale pyramid-structures on (100) surfaces of gold. The pyramids grew in a self-similar fashion with the facets aligned in (114) plane. Using the unique ...
Owing to its porous cellular structure and polymeric components, wood can be easily shaped in its transversal direction when it is heated and has sufficient water content. Thanks to this thermohydrous behaviour many manufacturing processes such as densific ...
Tensile properties and microstructure of Danocrystalline electrodeposited Ni at temperatures between room temperature and 330° C are presented. Above 300° C low flow stress and high tensile elongation are observed along with grain growth and segreg ...
Tensile tests have been carried out over a wide range of test speeds on compact tension specimens of polyamide 6 containing spherical silica particles, whose size and content had been adjusted to give optimum impact performance in conventional impact tests ...
Hot tearing, a severe defect occurring during solidification, is the conjunction of tensile stresses which are transmitted to the mushy zone by the coherent solid underneath and of an insufficient liquid feeding to compensate for the volumetric change. In ...