The influence of conditions of heat treatment of a solution [Zn(H2O)(O2C5H7)(2)] in 1-butanol (temperature 125-185 degrees C, treatment times 2, 4, and 6 h) on dispersion and microstructure of the formed nanocrystalline and poorly aggregated zinc oxide, pr ...