The origins of high hardening and low ductility in magnesium
Graph Chatbot
Chattez avec Graph Search
Posez n’importe quelle question sur les cours, conférences, exercices, recherches, actualités, etc. de l’EPFL ou essayez les exemples de questions ci-dessous.
AVERTISSEMENT : Le chatbot Graph n'est pas programmé pour fournir des réponses explicites ou catégoriques à vos questions. Il transforme plutôt vos questions en demandes API qui sont distribuées aux différents services informatiques officiellement administrés par l'EPFL. Son but est uniquement de collecter et de recommander des références pertinentes à des contenus que vous pouvez explorer pour vous aider à répondre à vos questions.
Modeling of the constitutive behavior was undertaken for Fe- Cr-C tempered martensitic alloys. Tensile tests were carried out at room temperature and constant nominal strain rate. In order to obtain a fully martensitic structure with different prior austen ...
The effects of neutron irradiation on austenitic stainless steels, usually used for the manufacturing of internal elements of nuclear reactors (e.g. the core shrouds), are the alteration of the microchemistry and the microstructure, and, as a consequence, ...
Irradiation is known to lead to a degradation of the mechanical properties of materials. This is particularly crucial in the case of materials that will be used in the future thermonuclear fusion reactor, where extremely high irradiation doses are expected ...
The present workshop dealt both theoretically and experimentally with issues of primary damage and irradiation induced defect evolution, helium and other impurities, dislocation-defect interactions, deformation to large plastic strains and fracture. It was ...
The irradiation of metals by energetic particles causes significant degradation of the mechanical properties(1,2), most notably an increased yield stress and decreased ductility, often accompanied by plastic flow localization. Such effects limit the lifeti ...
A detailed study of the strain-hardening on a Fe-9Cr-0.1C tempered martensitic model alloy has been undertaken in the temperature range of 77-343 K. The true stress-true strain curves were calculated from tensile test data. In the framework of a phenomenol ...
In situ cathodoluminescence experiments have been performed to follow the time dependence of the UV luminescence in epitaxial lateral overgrowth GaN specimens. The decrease of the observed intensity and red-shift of the UV peak are interpreted in terms of ...
We perform detailed finite element simulations of impact of metallic plates by spherical particles over a range of impact angles and speeds with a view to develop an insight into the fundamental mechanisms underlying solid-particle erosion. The particular ...
A high density of small defect clusters, similar to those observed in irradiated or quenched metals. has been observed in the deformed f.c.c. metals Cu, Au and Ni. The preliminary results show that the defect clusters are predominantly stacking fault tetra ...
We describe the first stage of the evolution of CL spectra, intensity and dislocation contrast under low keV electron beam for ELO-GaN with a low dislocation density. The UV and yellow intensities are decreased by beam irradiation. We have observed a broad ...