Scaling for hard-sphere colloidal glasses near jamming
Graph Chatbot
Chattez avec Graph Search
Posez n’importe quelle question sur les cours, conférences, exercices, recherches, actualités, etc. de l’EPFL ou essayez les exemples de questions ci-dessous.
AVERTISSEMENT : Le chatbot Graph n'est pas programmé pour fournir des réponses explicites ou catégoriques à vos questions. Il transforme plutôt vos questions en demandes API qui sont distribuées aux différents services informatiques officiellement administrés par l'EPFL. Son but est uniquement de collecter et de recommander des références pertinentes à des contenus que vous pouvez explorer pour vous aider à répondre à vos questions.
During solidification of metallic alloys, coalescence leads to the formation of solid bridges between grains or grain clusters when both solid and liquid phases are percolated. As such, it represents a key transition with respect to the mechanical behavior ...
Hot tearing is a major defect of solidification processes and welding. It occurs in metallic alloys while they are in the semi-solid state and is caused by a lack of liquid feeding in the mushy zone to compensate solid network openings due to tensile and s ...
A theory for the microscopic structure and the vibrational properties of soft sphere glass at finite temperature is presented. With an effective potential, derived here, the phase diagram and vibrational properties are worked out around the Maxwell critica ...
Composite sandwich panels comprising fibre reinforced polymer (FRP) skins and lightweight material cores are being increasingly used in civil engineering. In several applications, such as fa ades, roof structures and bridge decks, these panels may experien ...
Failure of amorphous solids is fundamental to various phenomena, including landslides and earthquakes. Recent experiments indicate that highly plastic regions form elongated structures that are especially apparent near the maximal shear stress Sigma(max) w ...
Silicon nitride based ceramics (SiAlONs); tetragonal polycrystalline zirconia (3Y‐TZP); alumina and their composites reinforced with different amount of multi‐ walled carbon‐nanotubes (CNTs) have been processed by Spark Plasma Sintering (SPS). High tempera ...
EPFL2013
Amorphous nanoparticles (a-NPs) have physicochemical properties distinctly different from those of the corresponding bulk crystals; for example, their solubility is much higher. However, many materials have a high propensity to crystallize and are difficul ...
American Association for the Advancement of Science2015
, , , ,
The influence of annealing between the Curie transition and the melting point of solvent cast polyvinylidene fluoride trifluoroethylene copolymer films on the crystalline structure, mechanical and electrical properties, and oxygen permeability is investiga ...
2014
,
Connectedness and applied stress strongly affect elasticity in solids. In various amorphous materials, mechanical stability can be lost either by reducing connectedness or by increasing pressure. We present an effective medium theory of elasticity that ext ...
The rigidity temperature of a solidifying alloy is the temperature at which the solid plus liquid phases are sufficiently coalesced to transmit long range tensile strains and stresses. It determines the point at which thermally induced deformations start t ...