Interplay between Process Zone and Material Heterogeneities for Dynamic Cracks
Graph Chatbot
Chattez avec Graph Search
Posez n’importe quelle question sur les cours, conférences, exercices, recherches, actualités, etc. de l’EPFL ou essayez les exemples de questions ci-dessous.
AVERTISSEMENT : Le chatbot Graph n'est pas programmé pour fournir des réponses explicites ou catégoriques à vos questions. Il transforme plutôt vos questions en demandes API qui sont distribuées aux différents services informatiques officiellement administrés par l'EPFL. Son but est uniquement de collecter et de recommander des références pertinentes à des contenus que vous pouvez explorer pour vous aider à répondre à vos questions.
We show that chevron-notched samples offer an attractive approach to the measurement of fracture toughness in micron-scale samples of brittle materials and use the method to characterize quartz and nanocrystalline alumina. Focused ion beam milling is used ...
Silicon nitride is a widely used industrial ceramic, specifically for dynamic loading applications because of its special mechanical and material properties. The investigation of the underlying mechanisms which lead to these properties is experimentally ch ...
The influence of slow crack growth in ceramics on the measurement of their fracture toughness under steadily increasing controlled load (as is generally practiced in microscale testing) is analyzed to identify conditions under which the phenomenon can caus ...
An experimental investigation is conducted to study the quasi-static and dynamic fracture behaviour of sedimentary, igneous and metamorphic rocks. The notched semi-circular bending method has been employed to determine fracture parameters over a wide range ...
Continuous-fiber ceramic matrix composites (CMCs) are of interest as hot-section components in gas turbine engines due to their refractoriness and low density relative to metallic alloys. In service, CMCs will be subjected to spatially inhomogeneous temper ...
Imperfections, like surface roughness and defects, introduced by common manufacturing processes are recognized to favor failure of microfabricated components and systems. Up to now only a reduced part of the ideal strength prediction by zero Kelvin quantum ...
Experiments and finite element simulations have been carried out to assess the warm pre-stressing effects on the effective fracture toughness of the high-chromium reduced activation tempered martensitic steel Eurofer97. The experiments have been conducted ...
The aim of the present thesis is to model numerically the dynamic failure behavior of concrete at the mesoscale. Concrete is the world's most widely used construction material and the structures made of it are subjected to dynamic loads during their long s ...
Using a spectral resolution of the elastodynamic boundary integral equations, this poster is presenting the effect of tougher heterogeneities along a planar fracture plane. A centered crack propagating along a 1-D heterogeneous interface under mixed-mode l ...
In the present work, LBE (lead-bismuth eutectic) embrittlement effects on ferritic/martensitic (FM) steels have been studied by conducting slow-strain-rate tensile (SSRT) testing on T91 and F82H steels either in Ar or in liquid LBE after irradiation to dos ...