Giorgio Margaritondo, Davor Pavuna, Mike Abrecht
We used pulsed laser deposition, with a Bi2Sr2CaCu2O8+x target, to grow films ranging from (1/4) to 10 unit cells thick. We studied these films, and reference Bi2Sr2CaCu2O8+x single crystal samples, using angle-integrated photoemission, core level photoemi ...
2002