DISCLAIMER: The Graph Chatbot is not programmed to provide explicit or categorical answers to your questions. Rather, it transforms your questions into API requests that are distributed across the various IT services officially administered by EPFL. Its purpose is solely to collect and recommend relevant references to content that you can explore to help you answer your questions.
The effect of reactor material (borosilicate and polyethylene terephthalate-PET) and its reuse on the microbiological and chemical decontamination of water by the photo-Fenton reaction at near-neutral pH was assessed. Escherichia coli was used as an indica ...
In this paper we experimentally investigate optical interactions between gold nanowires and fs-laser written waveguides in a view of applications for stationary-wave integrated Fourier-transform spectrometers in a movable mirror configuration. For this pur ...
Over the last decade, femtosecond lasers have been used extensively for the fabrication of optical elements via direct writing and in combination with chemical etching. These processes have been an enabling technology for manufacturing a variety of devices ...
The work presented in this paper deals with the bonding of small structures, down to 1 mu m. Its aim is to evaluate the dimensional limits of anodic bonding between silicon and pyrex 7740 glass. Test structures consisting in silicon pillars with controlled ...
During their lifetime, glass panels are repetitively exposed to thermal stresses. These thermal stresses result from temperature differences within the panel, which most notably cause the edges of the panels to be stressed in tension. When these thermal st ...
We report the fabrication of solenoidal microcoils with hollow core embedded within two 100 µm thick borosilicate glass wafers. The main process steps are the reactive ion etching of borosilicate glass, anodic wafer bonding, copper metal organic chemical v ...
The work presented in this paper deals with the bonding of small structures, down to 1 mu m. Its aim is to evaluate the dimensional limits of anodic bonding between silicon and pyrex 7740 glass. Test structures consisting in silicon pillars with controlled ...
This thesis explores transport phenomena in nanochannels on a chip. Fundamental nanofluidic ionic studies form the basis for novel separation and preconcentration applications for proteomic purposes. The measurements were performed with 50-nm-high 1D nanoc ...
We present the microfabrication and characterisation of a ball valve micropump in glass, which is magnetically actuated using the sinusoidal current of an external electromagnet. We employ the use of a simple powder blasting technology for microstructuring ...
We introduce powder blasting for the fabrication of glass microchips. Powder blasting is a fast and cheap technique with which we pattern channels in sodalime and pyrex glass with a width down to 100µm. We combine the technique with appropriate bonding pro ...