High-performance concretes from calcium aluminate cements
Graph Chatbot
Chat with Graph Search
Ask any question about EPFL courses, lectures, exercises, research, news, etc. or try the example questions below.
DISCLAIMER: The Graph Chatbot is not programmed to provide explicit or categorical answers to your questions. Rather, it transforms your questions into API requests that are distributed across the various IT services officially administered by EPFL. Its purpose is solely to collect and recommend relevant references to content that you can explore to help you answer your questions.
This dissertation originates from an investigation about the arising of the modern, German building expertise involving the use of concrete, which develops during the first three quarter of the 19th century against the backdrop of a general modernisation p ...
The water-absorption behavior of cement pastes (w/c=0.30) containing varying concentrations (i.e., 0, 0.2, and 5%) of a shrinkage-reducing admixture (SRA) was measured. Moisture ingress was monitored using X-ray absorption. A decrease in both the depth of ...
High-performance concrete is sensitive to early-age cracking, mainly due to its rapidly-developing autogenous shrinkage. Autogenous shrinkage and internal relative humidity (RH) decrease are direct consequences of the emptying of capillary pores due to cem ...
Durability and safety of concrete structures are fully governed by mechanical properties. This is especially true at early age, when cement matrix is not yet fully developed, and phase arrangement becomes critical for understanding mechanical behavior. Thi ...
At the turn of the 19th century, the production and use of concrete were limited by the unavailability of raw materials to produce good cement in several places. From that time onwards, the progress of chemistry and a number of empirical discoveries opened ...
A preliminary assessment of conditions for the industrial manufacture of a new cementitious system based on clinker-calcined clay and limestone, developed by the authors, referred as "low carbon cement" is presented. The new cement enables the substitution ...
Among different methods of measuring early age autogenous deformation of cementitious materials, the corrugated tube method described in the ASTMC1698-09 standard is one of the most commonly used. Despite the standardization and the common application of t ...
Calcareous fly ashes are high-potential reactive supplementary cementitious materials, which present an interesting alternative to slowly reacting siliceous fly ashes and to slags, which availability is more and more limited. Themain factor against an accu ...
Autogenous shrinkage is the unrestrained volume change of cementitious materials occurring at con-stant temperature without any change in mass. It occurs as a consequence of self-desiccation (de-crease of internal relative humidity) and increasing capillar ...
Alkali-activatedslag(AAS) binders are obtained by a manufacturing process less energy-intensive than ordinary Portland cement (OPC) and involves lower greenhouse gasses emission. These alkaline cements allow the production of high mechanical strength and d ...