Mechanical and microstructural integrity of nickel-titanium and stainless steel laser joined wires
Graph Chatbot
Chat with Graph Search
Ask any question about EPFL courses, lectures, exercises, research, news, etc. or try the example questions below.
DISCLAIMER: The Graph Chatbot is not programmed to provide explicit or categorical answers to your questions. Rather, it transforms your questions into API requests that are distributed across the various IT services officially administered by EPFL. Its purpose is solely to collect and recommend relevant references to content that you can explore to help you answer your questions.
The fracture strength of silicon nanowires grown on a [111] silicon substrate by the vapor-liquid-solid process was measured. The nanowires, with diameters between 100 and 200 nm and a typical length of 2 μm, were subjected to bending tests using an atomic ...
Virtual tensile experiments on cylindrical copper wires of nanometric diameter were carried out using molecular dynamics techniques based on the embedded-atom method. Transverse, atomically sharp surface cracks with circular fronts of different depths are ...
The effects of neutron irradiation on austenitic stainless steels, usually used for the manufacturing of internal elements of nuclear reactors (e.g. the core shrouds), are the alteration of the microchemistry and the microstructure, and, as a consequence, ...
In this study, the tensile and fracture properties and the microstructure of the reduced-activation tempered martensitic steel Eurofer97 have been investigated. This technical alloy is a 9%Cr steel developed within the European fusion material research pro ...
At small sizes, piezoelectric bending actuators are more practical and have more favorable downscaling properties than traditional electromagnets in the field of microfluidics. However, their application is limited by the difficulty of ensuring proper clam ...
Since decades traditional friction welding methods are applied industrially to metal and thermoplastic synthetics. Research showed that for different applications this method is promising for wood too. The process does not necessitate any additional materi ...
Three different approaches for metal to ceramic brazing are compared using the example of Si3N4/TiN-steel joints: the use of an active filler metal (single layer brazing system), the metallisation of the ceramic and brazing with a non active filler (two-la ...
For several decades friction welding technology has found broad application in many fields of the metal and plastic connection industry. The fabricated joints are laminar or punctiform depending upon the shape of the parts to be welded. The work presented ...
A new laser micro-spot welding procedure for copper has been developed in order to eliminate the shortcomings of existing techniques based on laser pulse shaping or in-situ temperature control. This procedure consists in dividing the welding process in fou ...
At the Chair of Timber Constructions of the Swiss Federal Institute of Technology in Lausanne (EPFL) tests were carried out to join wooden work pieces by friction welding without any additional welding deposit. It could be determined that this kind of tech ...