The main drawback of Ni/YSZ anode supports for solid oxide fuel cell application is their low tolerance to reducing and oxidizing (RedOx) atmosphere changes, owing to the Ni/NiO volume variation. This work describes a structured approach based on design of experiments for optimizing the microstructure for RedOx stability enhancement. A full factorial hypercube design and the response surface methodology are applied with the variables and their variation range defined as: (1) NiO proportion (40-60 wt% of the ceramic powders), (2) pore-former proportion (0-30 wt% corresponding to 0-64 vol.%), (3) NiO particle size (0.5-8 mu m) and (4) 8YSZ particle size (0.6-9 mu m).
Jan Van Herle, Stefan Diethelm, Philippe Aubin, Suhas Nuggehalli Sampathkumar, Maria del Mar Perez Fortes
, ,