Open-pore 99.99% pure Al and Al-5 wt.% Mg foam produced by replication, with pores either 400 or 75 gm in average diameter, are tested in compression with repeated relaxation cycles, at room temperature. Similar data are collected on pure aluminium. Estima ...
Elsevier2011