Prediction of Hot Tear Formation in Vertical DC Casting of Aluminum Billets Using a Granular Approach
Publications associées (39)
Graph Chatbot
Chattez avec Graph Search
Posez n’importe quelle question sur les cours, conférences, exercices, recherches, actualités, etc. de l’EPFL ou essayez les exemples de questions ci-dessous.
AVERTISSEMENT : Le chatbot Graph n'est pas programmé pour fournir des réponses explicites ou catégoriques à vos questions. Il transforme plutôt vos questions en demandes API qui sont distribuées aux différents services informatiques officiellement administrés par l'EPFL. Son but est uniquement de collecter et de recommander des références pertinentes à des contenus que vous pouvez explorer pour vous aider à répondre à vos questions.
Hot tear formation has been observed during the solidification of a succinonitrile–acetone (SCN-acetone) alloy by pulling the columnar dendrites in the transverse direction with a stick. It is observed that the cracking of the mushy zone (hot tears) always ...
A new criterion for the appearance of hot tears in metallic alloys is proposed. Based upon a mass balance performed over the liquid and solid phases, it accounts for the tensile deformation of the solid skeleton perpendicular to the growing dendrites and f ...
In order to eliminate internal and surface defects, which appear in the ingots during continuous casting of metallic alloys, homogeneous and fine structures are often required. Therefore, when the adjunction of inoculant substances is not possible, the ele ...
Mechanisms responsible for the embrittlement of leaded "free-machining" copper alloys at intermediate temperatures (i.e. around 400 °C) are examined using a combination of microstructural and mechanical characterization. Tensile tests are conducted on pure ...
Semi-continuous direct-chill (DC) casting of aluminium ingots suffers from a very frequent defect which can lead to a strong decrease in productivity: hot tearing. This phenomenon takes place in the mushy state (i.e., at solid fractions, gs, lower than uni ...
As for most of the topics in the field of solidification, Mert Flemings has always pioneered new ideas. While much of the understanding of hot tearing formation was already known about 30 years ago, he devised with Metz an interesting apparatus for studyin ...
As for most of the topics in the field of solidification, Mert Flemings has always pioneered new ideas. While much of the understanding of hot tearing formation was already known about 30 years ago, he devised with Metz an interesting apparatus for studyin ...
While studies of solidification microstructures have focused mainly on the tips of the dendrites, the last stage solidification is equally important from the point of view of defect formation (porosity, hot tearing), mechanical strength build-up and precip ...
We report findings of large metal grains (~150 um) with distinct zoning patterns in Ni, Co, Cr, and Si in CH chondrites which are consistent with a condensation origin from a gas of solar composition. ...