Correlation of microdistortions with misfit volumes in High Entropy Alloys
Graph Chatbot
Chattez avec Graph Search
Posez n’importe quelle question sur les cours, conférences, exercices, recherches, actualités, etc. de l’EPFL ou essayez les exemples de questions ci-dessous.
AVERTISSEMENT : Le chatbot Graph n'est pas programmé pour fournir des réponses explicites ou catégoriques à vos questions. Il transforme plutôt vos questions en demandes API qui sont distribuées aux différents services informatiques officiellement administrés par l'EPFL. Son but est uniquement de collecter et de recommander des références pertinentes à des contenus que vous pouvez explorer pour vous aider à répondre à vos questions.
Five different grain sizes are produced in 0.17 wt% carbon steel using varying rates of cooling from austenitization temperatures. Controlled furnace cooling from 1100 °C and 950 °C produces coarse ferrite grains of 40 µm and 32 µm diameter, respectively, ...
The aim of the thesis is to obtain more understanding about the influence of plastic deformation on the microstructural changes observed in single crystal (SX) Ni-based superalloys using diffraction techniques. This work was organised around two main probl ...
Ingots of an oxide dispersion strengthened reduced activation ferritic steel with the Fe-14Cr-2W-0.3Ti-0.3Y(2)O(3) chemical composition (in wt.%) were synthesized by mechanical alloying of elemental powders with 0.3 wt.% Y2O3 particles in a planetary ball ...
An argon gas atomized, pre-alloyed Fe-14Cr-2W-0.3Ti (wt.%) reduced activation ferritic (RAF) steel powder was mechanically alloyed with 0.3wt.% Y2O3 nano-particles in an attritor ball mill and consolidated by hot isostatic pressing at 1150 °C under a press ...
Copper and copper alloys typically experience a sharp loss in ductility at intermediate temperature, induced by grain boundary damage and fracture processes. The susceptibility of the material to intermediate temperature embrittlement is, as a result, stro ...
Six oxide dispersion strengthened (ODS) ferritic steels, with the composition of Fe-(12-14)Cr-2W-(0.1-0.3-0.5)Ti-0.3Y(2)O(3) (wt.%), have been prepared by mechanically alloying elemental powders of Fe, Cr, W, and Ti with Y2O3 nano-particles followed by hot ...
Trans Tech Publications Ltd, Laublsrutistr 24, Ch-8717 Stafa-Zurich, Switzerland2009
In the quest of materials for the first wall of the future fusion reactor, it has been shown that oxide dispersion strengthened (ODS) ferritic / martensitic (F/M) steels appear to be promising candidates. The inherent good mechanical properties supported b ...
Secondary gamma' precipitation in a commercial single crystal Ni-based superalloy after the 1100 degrees C isothermal aging has been investigated by atom probe tomography. After the isothermal aging for 300 s, 1800 s and 3600 s, a bimodal size distribution ...
Dry, compression molded films of medical grade poly-L-lactide (PLLA) showed a marked reduction in tensile strength and strain after accelerated ageing in aqueous NaOH at 50 degrees C. accompanied by mass loss, surface erosion, increased hydrophilicity and, ...
The paper presents the microstructure and mechanical properties of an oxide dispersion strengthened (ODS), reduced activation, ferritic steel, namely the Fe-14Cr-2W-0.3Ti-0.3Y(2)O(3) alloy, which was fabricated by hot isostatic pressing followed by high sp ...