Effect of tool travel and rotation speeds on weld zone defects and joint strength of aluminium steel lap joints made by friction stir welding
Related publications (36)
Graph Chatbot
Chat with Graph Search
Ask any question about EPFL courses, lectures, exercises, research, news, etc. or try the example questions below.
DISCLAIMER: The Graph Chatbot is not programmed to provide explicit or categorical answers to your questions. Rather, it transforms your questions into API requests that are distributed across the various IT services officially administered by EPFL. Its purpose is solely to collect and recommend relevant references to content that you can explore to help you answer your questions.
Nanostructure ZnO hollow microspheres with average crystallite size of about 15 nm, and average diameters of about 1 mu m, were successfully fabricated through a novel hydrothermal method. Hollow microspheres were formed due to self-assembly of ZnO oblong ...
The microstructure, chemical and phase composition of the hard Ni-P-Ti layer formed on the Ti-6Al-4V alloy after duplex surface treatment were investigated by light microscopy, X-ray diffraction, scanning electron microscopy and analytical/high-resolution ...
The effects of neutron irradiation on austenitic stainless steels, usually used for the manufacturing of internal elements of nuclear reactors (e.g. the core shrouds), are the alteration of the microchemistry and the microstructure, and, as a consequence, ...
This work presents the preliminary results on application of mineral sacrificial layer that is prepared to structure LTCC (low temperature co-fired ceramic). The proposed method suggests utilization of a sacrificial paste, which remains "permanent" during ...
The template method was used for preparing Zn1-xCoxO nanowires with x ranging from 0.01 to 0.05. Thus, electrochemical deposition was employed for filling up the pores of polycarbonate ion track nanoporous membranes with the desired material. The method al ...
Institute of Electrical and Electronics Engineers2008
The fabrication procedure changes when changing the size of the structural components. For the weldments, the change of the welding procedure leads to the change in residual stresses which consequently affects the fatigue life of the structure. The weld si ...
Be has a tendency to form particularly brittle intermetallics with Cu and a lot of other elements. Insertion of interlayers may be a solution to increase bond quality. Ion Beam Analysis (IBA) methods have been considered together with scanning electron mic ...
Syntheses of ZSM-5 coatings on stainless steel plates were carried out via the substrate heating method. The reaction mixture was kept at temperatures below 100 °C, while the metal plates were heated to temperatures above 100 °C. It was demonstrated that c ...
For several decades friction welding technology has found broad application in many fields of the metal and plastic connection industry. The fabricated joints are laminar or punctiform depending upon the shape of the parts to be welded. The work presented ...
Nickel-Titanium (NiTi) shape memory alloys are often used in medical component devices, for instance as guide wires for neurological surgery applications. The manufacture of such devices becomes more and more challenging, especially considering the need to ...