Fracture toughness testing of nanocrystalline alumina and fused quartz using chevron-notched microbeams
Graph Chatbot
Chat with Graph Search
Ask any question about EPFL courses, lectures, exercises, research, news, etc. or try the example questions below.
DISCLAIMER: The Graph Chatbot is not programmed to provide explicit or categorical answers to your questions. Rather, it transforms your questions into API requests that are distributed across the various IT services officially administered by EPFL. Its purpose is solely to collect and recommend relevant references to content that you can explore to help you answer your questions.
As a second part of this series, the present study also addresses the water resistance of joints obtained by friction welding. Here, the mode II fracture is in focus, that is, 4-points end-notched flexure specimens (4-ENF) were investigated with various mo ...
The edge strength of glass is affected by the load history. To quantify this effect, 12 series of glass specimens were subjected to either linearly increased (reference value), constant or cyclic loading. For constant loading the experimental values could ...
Effects of non-uniform strains on tensile fracture of fiber-reinforced ceramic–matrix composites have not been satisfactorily explained by existing mechanics-based models. In this paper, we use an exact model of fiber fragmentation under global load sharin ...
Fracture experiments in a notched semi-circular bend configuration were conducted to characterize rate effects and failure micromechanisms of a marble using a servo-hydraulic machine and a modified split Hopkinson pressure bar. Three real-time measurement ...
Fracture toughness tests are conducted at room temperature and 923 K (650 degrees C) on SENB (Single Edge Notched Bend) specimens of three different (alpha(2) + gamma ) TiAl-based alloys. One alloy is a conventional near fully lamellar Ti-45Al-2Mn-2Nb + 0. ...
The microstructure and mechanical properties of hot rolled Fe-40 at-%Al based intermetallic alloys, with 0.1 at-%Zr and different additions of B (varying from 0.01 to 0.1 at-%), are characterised. The additions of Zr and B improve tensile properties at roo ...
In this work we have studied brittle fracture in high-chromium reduced activation tempered martensitic steels foreseen as structural materials for thermonuclear fusion reactors. Developing the adequate materials that can withstand the severe irradiation co ...
Elastoplastic toughness testing of pure aluminium replicated foam is conducted following a J-procedure adapted from the ASTM E1820-08a standard using disc-shaped compact tension specimens. Tests cover a wide range of foam relative density V-m (10-24%). Res ...
Mechanical properties of nanostructures could be remarkably different from their bulk counterparts owing to scale effects, which have attracted considerable research interest in recent years. However, nanomechanics studies are hindered by the difficulties ...
The Mode I and II fracture behaviors of adhesively-bonded joints composed of pultruded glass fiber-reinforced polymer (GFRP) laminates were experimentally investigated using Double-Cantilever-Beam (DCB) and End-Loaded-Split (ELS) specimens. The large speci ...