Comportement structural des bétons de fibres ultra performants en traction dans des éléments composés
Graph Chatbot
Chattez avec Graph Search
Posez n’importe quelle question sur les cours, conférences, exercices, recherches, actualités, etc. de l’EPFL ou essayez les exemples de questions ci-dessous.
AVERTISSEMENT : Le chatbot Graph n'est pas programmé pour fournir des réponses explicites ou catégoriques à vos questions. Il transforme plutôt vos questions en demandes API qui sont distribuées aux différents services informatiques officiellement administrés par l'EPFL. Son but est uniquement de collecter et de recommander des références pertinentes à des contenus que vous pouvez explorer pour vous aider à répondre à vos questions.
In anticipation of the introduction of high modulus materials in the Swiss standards, a research project has been carried out for the evaluation of these bituminous mixtures. Three full-size test sections were built in a test hall for ALT named Halle-fosse ...
The reinforcement potential of pulp fibres is presently not fully explored in thermoplastic composites. One of the reasons is that currently used processing methods comprise several severe thermomechanical steps inducing premature degradation of the fibres ...
The mechanical properties of continuous fibre reinforced metals (CFRMs) are known to be very sensitive to the selection and composition of the metallic matrix; for aluminium based CFRMs, commercial alloys are not suitable for this purpose. In the present s ...
The paper presents a study on the tensile behavior of UHPC conducted at the structural concrete laboratory at the Swiss Federal Institute of Technology in Lausanne (EPFL). Material tests and tests on structural members with reinforcement bars have been per ...
International Symposium on Ultra High Performance Concrete2004
The results of the investigation on durability of vegetable fibre-mortar composites subjected to three different environmental conditions; immersed in water, exposed to the open air weathering and controlled cycles of wetting and drying are presented in th ...
In many casting processes, some stages, such as the starting phase in the direct chill casting of aluminium alloys, are particularly critical because of the propensity of some alloys to develop either hot tears which initiate at non zero liquid fraction, o ...
Advanced Cementitious Materials such as HPFRCC are well adapted for durable repair and strengthening of concrete structures. Experimental and numerical investigations have been conducted to study the behavior of hybrid structural elements consisting of HPF ...
Pre-stress bonded composite patch is a promising technique to reinforce steel member damaged by fatigue. ifhe effectiveness of this technique was verified by fatigue tests on notched steel plates. Results showed that the application of carbon fibre reinfor ...
The dimensional stability of V-shaped composite parts made from polyamide-12/carbon fibre (PA12/CF) commingled yarn has been studied. An anisotropic, thermoviscoelastic material model was implemented in a finite element solver to predict the internal stres ...
Hot tear is one of the most serious defect which a casting can suffer. It represents a major limitation to the production of foundry cast parts and to the productivity of continuous casting processes such as the direct chiil casting of aluminium alloys. As ...